APPLICATION NOTE
DISCUSSION
SIMS is a powerful analytical technique which allows detection of all elements from H to U with excellent sensitivity. The table provides a list of typical detection limits for impurities in a HgCdTe matrix for normal depth profiling conditions. Lower detection levels can be obtained for many species under optimal analytical conditions on a case-by-case situation.